名称 | 密度 | 成型收缩率 | UL94阻燃 | 产品描述及应用 | 产品实例 |
PA612 158 | 1.06 | UL746B/0.75mm | 耐水解,耐热性,中等粘度,聚酰胺树脂 |
![]() |
||
PA612 151 | 1.06 | UL746B/0.75mm | 耐水解,耐热性,低粘度 |
![]() |
||
PA1010 RS LC1610 | 105 | 挤出成型,增韧,热稳定,含有75%的再生来源成分 |
![]() |
|||
PA1010 RS LC1600 | 1.04 | UL94 HB | 挤出成型,含有60%的再生来源成分,柔性,增韧, |
![]() |
||
PA1010 RS LC1201 | 1.04 | UL94 HB | 挤出成型,含有85%再生来源成分,灵活的再生聚酰胺树脂,中等粘度, |
![]() |
||
PA1010 RS LC1010 | UL94 HB | 挤出成型,含有90%的再生来源成分,柔性,未增强 |
![]() |
|||
PA1010 RS LC1000 | UL94 HB | 挤出成型,含有90%的再生来源成分,柔性,未增强 |
![]() |
|||
PA6 PLS93G35DH1 | 1.4 | UL94 HB | 注塑成型,含有35%玻璃钎维增强,优良的耐热性 |
![]() |
||
PA6 FN727 | 1.02 | UL94 HB | 非常灵活的聚酰胺6具有良好的低温合金树脂 |
![]() |
||
PA6 EFE7374 | 1.41 | UL94 HB | 注塑成型,含有40%钎维增强,热稳定,润滑,增韧 |
![]() |
||
PA6 BM73G15P | 1.22 | UL94 HB | 吹塑成型,含有15%玻璃钎维增强,热稳定,润滑,增韧 |
![]() |
||
PA6 7335F | 1.13 | UL94 HB | 注射成型,润滑,聚酰胺6树脂 |
![]() |
||
PA6 7331J | 1.13 | UL94 HB | 注射成型,润滑快速循环聚酰胺6树脂 |
![]() |
||
PA6 7304 | UL94 HB | 挤出成型,中等粘度,无润滑尼龙6树脂 |
![]() |
|||
PA6 84G33 | UL746B/0.75mm | 含有33%玻璃钎维增强增韧聚酰胺66和聚酰胺6合融黑色立方体混合树脂。这种树脂是 |
![]() |
|||
PA6 74G33W | 1.39 | UL94 HB | 高光泽汽车耐候黑色,含有33%玻璃纤维增强,尼龙适用于汽车,家具,家用电器 |
![]() |
||
PA6 74G33J | UL94 HB | 含有33%玻璃钎维增强,
尼龙66和尼龙6的熔融树脂,适用于汽车,家具,家用电器 |
![]() |
|||
PA6 73M40 | 1.45 | UL746B 0.75mm | 注塑成型,含有40%的矿物增强,热稳定,低翘曲 |
![]() |
||
PA6 73M30 | UL746B 0.75mm | 注塑成型,含有30%矿物增强,热稳定,低翘曲 |
![]() |
|||
PA6 73GM40 | 1.46 | UL94 HB | 含有40%矿物/玻璃纤维增强,热稳定尼龙6树脂注塑成型 |
![]() |
||
PA6 73G15HSL | 1.25 | UL746B 1.5mm | 含有15%玻璃纤维增强,热稳定,黑色尼龙6树脂注塑成型.. |
![]() |
||
PA RS LC4601 | 1.04 | UL94 HB | 挤出成型,良好的灵活性,聚酰胺树脂 |
![]() |
||
PA RS LC2800 | UL94 HB | 挤出成型,含有至少60%的可再生来源的成分(重量)的可再生来源的聚酰胺。它是一个 |
![]() |
|||
pa RS LC2600 | 1.05 | UL94 HB | 含有50%以上的可再生来源成分 |
![]() |
||
PA PLSFR95G15DH2 | 1.48 | UL94 HB | 含有15%玻璃纤维增强,阻燃,适用于电器,电子 |
![]() |